Skip to main content

Advertisement

Table 2 Parameters for Eq. (1) of the proposed model

From: Mechanical properties of High and Very High Steel at elevated temperatures and after cooling down

parameter k y k u k E
a1 −85.81 0.9878 0.1871
b1 184.4 40.68 −12.96
c1 297.7 469.1 132
a2 86.73 0.3482 0.9199
b2 184.2 437.9 181.6
c2 299.8 205.9 483.9