Figure 19From: Overview of aluminum alloy mechanical properties during and after firesHardening rates (dσ/dε) of (a) 5083-H116 and (b) 6061-T651 calculated from the true stress-logarithmic DIC strain relations for specimens previously exposed at 20°C/min.Back to article page